Outperforms and outlasts ordinary galvanised steels, painted or unpainted Age: 17 years
The post-painted (field painted) hot-dip galvanised roof section is in poor condition, and even perforated at a few points. The 55% Al-Zn section, though dirty, is in good condition - apart from localised corrosion due to pollution from the roof stack. Age: 23 years
The performance of 55% Al-Zn on the 23-year-old roof contrasts sharply with the deterioration of the roof vent in hot-dip galvanised steel. Age: 18 years
The 18-year-old 55% Al-Zn roof on the right (rural environment, UK) contrasts with galvanised panels at the same location, beginning to rust after only 6 years. Age: 20 years
The galvanised fastener on this 20 year old
panel in an urban environment has rusted, and the 55% Al-Zn material is
starting to sacrifice itself to protect the fastener. |
|